KUAT TEKAN BETON DENGAN PENAMBAHAN LIMBAH PECAHAN BATU SILIKA SEBAGAI SUBTITUSI AGREGAT KASAR

Muktasid, Luqman (2023) KUAT TEKAN BETON DENGAN PENAMBAHAN LIMBAH PECAHAN BATU SILIKA SEBAGAI SUBTITUSI AGREGAT KASAR. Sarjana (S1) thesis, Universitas Islam “45” Bekasi.

[thumbnail of PENDAHULUAN.pdf] Text
PENDAHULUAN.pdf

Download (432kB)
[thumbnail of BAB I.pdf] Text
BAB I.pdf
Restricted to Repository staff only

Download (18kB) | Request a copy
[thumbnail of BAB II.pdf] Text
BAB II.pdf
Restricted to Repository staff only

Download (716kB) | Request a copy
[thumbnail of BAB III.pdf] Text
BAB III.pdf
Restricted to Repository staff only

Download (879kB) | Request a copy
[thumbnail of BAB IV.pdf] Text
BAB IV.pdf
Restricted to Repository staff only

Download (834kB) | Request a copy
[thumbnail of BAB V.pdf] Text
BAB V.pdf
Restricted to Repository staff only

Download (117kB) | Request a copy
[thumbnail of DAFTAR PUSTAKA.pdf] Text
DAFTAR PUSTAKA.pdf

Download (207kB)

Abstract

The increasing number of glass and bottle factories in Indonesia that use
refractory stone furnaces and produce waste, one of which is silica bricks, where
these bricks are used as smelting furnaces. To avoid the accumulation of waste,
silica stone is used as a substitute for gravel in concrete mixtures in an effort to
increase its compressive strength.
This study aims to determine the ratio of compressive strength of normal
concrete (0% silica stone fragment waste) with substitution variations of 5%, 15%,
and 25% Silica Rock Fractional Waste (LPBS). Concrete compressive strength
testing based on SNI 03-6825-2002 using a Compression Test Machine with a
capacity of 1500 kN with ASTM C-39 test standards.
The results showed that the composition of the concrete mixture at the age of
28 days with a variation of 0% LPBS (normal concrete) with an average
compressive strength of 210.643 kg/cm² or 20.6573 MPa. For LPBS variations, 5%
gives a maximum average compressive strength of 231.3504 (Kg/cm2) or 22.6880
(MPa). For LPBS variations, 15% gives a maximum average compressive strength
of 239.2049 (Kg/cm2) or 23.4583 (MPa). For LPBS variations, 25% gives a
maximum average compressive strength value of 260.6261 (Kg/cm2) or 25.5591
(MPa). 5. With the results of this test, it can be concluded that concrete with a
mixture of 5%, 15%, and 25% silica stone fragment waste at the age of 28 days is
able to increase the compressive strength value of concrete against the compressive
strength of normal concrete.
Keywords: Concrete, Strong compressive, Silica.

Item Type: Thesis (TA, Skripsi, Tesis, Disertasi) (Sarjana (S1))
Contributors/Dosen Pembimbing,NIDN Dosen bisa diakses di LINK https://bit.ly/NIDNdosenunismabekasi:
Contribution
Contributors / Dosen Pembimbing
NIDN
UNSPECIFIED
Paryati, Ninik
0429017903
UNSPECIFIED
Prihesnanto, Fajar
0405017008
Keywords / Kata Kunci: Kata kunci: Beton, Kuat tekan, Silika
Subjects: Manajemen Konstruksi
Faculty: Fakultas Teknik > Teknik Sipil S1
Depositing User: Mr Luqman Muktasid
Date Deposited: 15 Aug 2023 09:14
Last Modified: 15 Aug 2023 09:14
URI: http://repository.umindonesia.ac.id/id/eprint/3672